PCB trace resistance/heating calculator

1 oz copper is taken as 35 μm (1.378 mil). Changing the width or length unit reinterprets the number; changing the thickness unit converts it. To include self-heating, add the estimated rise to the ambient temperature and enter that as the copper temperature.

Enter the trace width and length to see its resistance.

No valid result to draw.

Show the steps

Interactive calculation is unavailable until JavaScript loads. The formulas, worked examples and references below remain available.

Calculate the resistance, voltage drop and power loss of a PCB trace from its width, length and copper thickness, and estimate its IPC-2221 temperature rise.

How to use

Enter the trace width and length with their units.

Enter the copper thickness as ounces, μm or mil, and the copper temperature.

Enter the current, and choose external or internal layer for the temperature rise.

Read the resistance, sheet resistance, voltage drop, power and the IPC-2221 temperature rise.

Copy result copies labeled values; Reset restores the starting fields.

Science

A trace is a flat copper conductor, so its resistance is the copper's resistivity times the length divided by the cross-section, width times thickness. Annealed copper is 1/58 Ω mm2/m at 20 °C, and resistance rises 0.393 % per °C.

Board designers often count squares: a square of copper of any size has the same resistance, the sheet resistance ρ / t. For 1 oz (35 μm) copper at 20 °C that is about 0.49 mΩ per square, and a trace's resistance is that times its length divided by its width.

The power dissipated is I^2 × R. How hot that makes the trace depends on how it sheds heat. The IPC-2221 first-pass relation I = k × ΔT^0.44 × A^0.725, solved here for ΔT, gives the rise above ambient: k = 0.048 for outer layers and 0.024 for inner layers, so an inner trace runs about 4.8 times hotter by this estimate.

IPC-2152 (2009) replaced the old charts with measurements that include board thickness, planes and vias, and it often predicts cooler inner traces. Treat the rise as a first pass and check hot traces with IPC-2152 or a thermal simulation.

Limitations: DC resistance with IACS annealed copper and a uniform rectangular cross-section; real foil, plating on outer layers, etch undercut and solder change it by a few percent or more. The copper temperature is entered, not solved from the rise. The rise is an empirical fit to still-air charts for a single trace, valid up to 35 A, 400 mil, 10 to 100 °C and 0.5 to 3 oz, and the tool flags anything outside that range. It does not give the width needed for a current (the trace-width calculator does) and is not a fusing rating.

Formulas

Resistivity: ρ = (1/58) × (1 + 0.00393 × (T - 20)) Ω mm2/m.

Resistance: R = ρ × L / (W × t), with L in m and W, t in mm.

Sheet resistance: R_sq = ρ / t; R = R_sq × L / W.

Drop and power: V = I × R; P = I^2 × R.

Temperature rise: ΔT = (I / (k × A^0.725))^(1/0.44), A in mil2, k = 0.048 external, 0.024 internal.

Examples

10 mil wide, 100 mm long, 1 oz, 20 °C, 1 A, external: 193.9 mΩ; 193.9 mV; 193.9 mW; rise 13.2 °C. 0.4926 mΩ per square × 393.7 squares; A = 13.78 mil2.

Same trace on an internal layer: rise 63.7 °C. Common mistake: using the outer-layer estimate inside the board; k halves and the rise grows 4.8 times.

1 mm wide, 50 mm long, 1 oz, 20 °C, 3 A, external: 24.63 mΩ; 73.89 mV; 221.7 mW; rise 16.7 °C. 50 squares of 0.4926 mΩ.

100 mil wide, 4 in long, 2 oz, 60 °C, 5 A, external: 11.4 mΩ; 57 mV; 285 mW; rise 3.67 °C, below the lowest chart curve. ρ at 60 °C = 0.019952 Ω mm2/m over 0.1778 mm2.

0.3 mm wide, 100 mm long, 1 oz, 85 °C, 1 A: 206.1 mΩ. Boundary of a hot board: the same trace at 20 °C is 164.2 mΩ.

References

NBS Handbook 100: Copper Wire Tables

OpenStax: Resistivity and resistance

Advanced Circuits: trace width calculator (IPC-2221 constants)

IPC-2152 table of contents